Print failed because the layer adhesion is shit on my printer.

  • GregorTacTacOP
    link
    fedilink
    English
    27 months ago

    A lot of printing. It’s basically impossible to clean it well.

    • AmbiguousProps
      link
      fedilink
      English
      27 months ago

      Are you removing your prints when the build plate is still hot? If so, and your plate is PEI, it’ll get destroyed

      • @[email protected]
        link
        fedilink
        English
        27 months ago

        It looks like a glass carborundum Creality plate. I have one of them, they work really well until one day they just don’t.

        • GregorTacTacOP
          link
          fedilink
          English
          37 months ago

          I second that. Mine worked for quite a bit of time until it stopped working properly.

          • @[email protected]
            link
            fedilink
            English
            17 months ago

            Glue stick helps, as does cleaning with ISO between every. single. print. Also praying.

            I got an old school build-tak style sticker for one of my glass beds once I finally got sick of it. Ender 3 style glass beds are just bizarre, ornery little things.

            • @[email protected]
              link
              fedilink
              English
              27 months ago

              Buildtak is fantastic, I’ve swapped over to all buildtak on my voron and for abs on my prusa, A little bit of 99ipa between prints and you’re good, never had to worry about adhesion. I had a glass bed on a Mendel Max 2 literally a decade ago that I ended up selling about a year later when I moved cross country, ignoring bed leveeling and z axis issues I had, adhesion was always a mess, ended up doing the coat in polyimide tape and gluestick thing with success but it was always a bit how you doing. It’s great how far things have come.

    • @[email protected]
      link
      fedilink
      English
      17 months ago

      With that one (creality textured glass carborundum something or other) I kept hitting it with 95%+ IPA, it just gives out eventually. I switched to a textured spring steel plate recently, world of difference for petg, PLA, and tpu. It’s just another consumable :/

      If you’re not ready to switch yet a layer of masking tape can get you by for awhile, it’s just a pain because the masking tape will need to be replaced about every other print depending on your settings.