• mattaw@lemmy.world
    link
    fedilink
    English
    arrow-up
    0
    ·
    edit-2
    2 years ago

    I could not get a 0.6 to stop oozing and stringing with petg and pla. Just couldn’t so switched back to 0.4. Dragon hot end w. Bowden tube after titan extruder.

    • jtablerd@lemmy.worldOP
      link
      fedilink
      English
      arrow-up
      1
      ·
      2 years ago

      can’t believe it - I was stringing and clogging with 0.4 (likely trouble with retraction but tuned to hell and back) but running same parts at 0.8 (granted not detailed, but functional big parts) without stringing, same retraction settings, and 40% print time it’s wild